Materialia | 2019

Effects of Fe concentration on helium bubble formation in NiFex single-phase concentrated solid solution alloys

 
 
 
 
 
 
 
 
 
 

Abstract


Abstract The formation of helium bubbles and the consequential property degradation are critical challenges for materials used in advanced nuclear energy systems. The mechanism of helium bubble formation in a series of NiFex (x\u202f=\u202f0, 20, 35, or 50 at.%) single-phase concentrated solid solution alloys (SP-CSAs) are studied in this work. Transmission electron microscopy analysis shows that with increasing Fe concentration, the average bubble size decreases while the bubble number density increases, indicating the growth of large helium bubbles in NiFex SP-CSAs is suppressed by increasing the alloy chemical complexity through increased Fe concentration. Mechanisms for the slower bubble growth rate in NiFex binary SP-CSAs compared Ni are identified. These mechanisms include promotion of Frenkel pair recombination, denser and more homogeneously distributed nucleation sites, and increased helium atom densities inside the bubbles. The results demonstrate that optimizing the chemical complexity in SP-CSAs can be an effective approach to design materials with superior resistance to helium bubble nucleation and growth.

Volume 5
Pages 100183
DOI 10.1016/J.MTLA.2018.100183
Language English
Journal Materialia

Full Text